Fiji® series is a modular, high-vacuum ALD system that accommodates a wide range of deposition modes using a flexible architecture and multiple configurations of precursors and plasma gases. The result is a next-generation ALD system capable of performing thermal and plasma-enhanced deposition.

Fiji's advanced features include:

  • Proprietary Chamber Turbo Pumping System
  • Improved Plasma Design
  • Ergonomic Operator Interface
  • In-Situ Ellipsometry
  • In-Situ Quartz Crystal Microbalance
  • Integrated Ozone
  • Glove Box Interface

The Fiji® is available in several different configurations, including Dual Chamber and Load Lock. Each chamber can be configured with up to six precursor lines that can accommodate solid, liquid or gas precursors, and six plasma gas lines, offering significant experimental flexibility in a compact and affordable footprint.

Technical specifications

Operational Modes Continuous Mode™ (Traditional Thermal ALD) 
Exposure Mode™ (High Aspect Ratio ALD) 
Plasma Mode™ (Plasma-Enhanced ALD)
Substrate Size Up to 200 mm
Substrate Temperature 500°C 200mm substrate heater standard 
800°C 100mm substrate heater optional
Deposition Uniformity σ Uniformities 
Thermal Al2O3 – 1.5% 
Plasma Al2O3 – 1.5%
Precursors 4 precursor lines standard, up to 6 optional 
Gas, liquid, or solid precursors individually heatable to 200°C 
Industry standard high speed ALD valves (10ms minimum pulse time) 
Widely available 50cc (25mL fill max) stainless steel precursor cylinders
Gases 100 sccm Ar precursor carrier gas MFC 
200 sccm Ar plasma gas MFC 
100 sccm N2 plasma gas MFC 
100 sccm O2 plasma gas MFC 
100 sccm H2 plasma gas MFC
Trap Integrated, heated, thin foil ALD trap
Compatibility Clean Room Class 100 Compatible
Compliance CE, TUV, FCC
Dimensions F200: 
1600 x 715 x 1920 mm 
F200 with load lock: 
1845 x 715 x 1920 mm
Power 220-240 VAC, 4200 W per reactor (excludes pump)
Control Microsoft Windows™ 7 Laptop PC, LabView based system control
Vacuum Pump >50CFM dry pump required 
Available or customer supplied
System Options Spectroscopic Ellipsometer Ports 
Quartz Crystal Microbalance 
RGA Port 
Optical Emission Spectrometer 
Wafer Plus 
Ozone Generator 
Low Vapor Pressure Deposition 
Glove box Interface 
Load Lock